China
China
Gulf
Pakistan
Iran
Russia
WeChat/WhatsApp/Mob +86 18724717692 Email: sales@monsterbelting.com
WeChat/WhatsApp/Mob +97165231717 Address : P8-08-44, P.O Box. 513642, Sharjah Airport International Free Zone, United Arab Emirates.
WeChat/WhatsApp/Mob +92-51-2361407 IAS Trade Zone (Pvt) Ltd. is our Exclusive agency in Pakistan.
WeChat/WhatsApp/Mob +98 313 531 5580 – 82 Address: Isfahan Province, Isfahan, Khorasgan, Arghavanieh Blvd, Iran
WeChat/WhatsApp/Mob +7 (926) 734-96-63 Russian Federation, Moscow
Ceritified
ISO 9001:2008
The Best
#1 in China
Number #1
Suplier in region
Get A Quote

High Temperature Resistance Conveyor Belt

High Temperature Resistance Conveyor Belt

heat resistance belt

High Temperature Resistance Conveyor Belt  is made of cotton canvas or polyester canvas and cover rubber with heat resistant.Be used to convey hot materials or elevated temperature materials such as metallurgy, casting, coking, building material, chemical and so on. Because the cover rubber is of a certain heat resistance.

Standard:

GB/T20021-2005《High Temperature Resistance Conveyor Belt》

Applicationfields:

Metallurgy, steel plant, building material and construction, energy, chemical,machinery equipment and port.

Tensilestrength:

500~3000N/mm

Width:

500~2400mm

Heat-Resistance-Bucket-Elevator-Conveyor-Belt-with-Steel-Cord-in-Cement-Plant
Coal Feeder Used Flange Conveyor

Characteristics:

1、Heat-resistant cover resists cracking and hardening
2、High-temperature resistance to tearing and abrasion
3、High strength carcass construction
4、The carcass with heat-resistant material

High Temperature Resistance Conveyor Belt Type:

T1: It can stand the experimental temperature of no more than 100℃, symbols as T1
T2: It can stand the experimental temperature of no more than 125℃, symbols as T2
T3: It can stand the experimental temperature of no more than 150℃, symbols as T3
T4: It can stand the experimental temperature of no more than 175℃, symbols as T4

After the high temperature resistance belt heating test,its physical and mechanical performance should be in accordance with the provisions below.

Item Type
T1 T2 T3 T4
Variation Range
Hardness Difference betweenbefore and after aging(1RHD) +20 +20 ±20 ±20
Maximum value after aging (1RHD) 85
Tensile Strength Performance Change Rate,% -25 -30 -40 -40
Minimumvalue after aging ,Mpa 12 10 5 5
Elongation Change Rate after aging ,% -50 -50 -55 -55
Minimumvalue after aging,% 200 200 180 180